Petrobond or?

Discussion in 'Home Foundry & Casting Projects' started by dkwflight, Jul 13, 2018 at 6:51 PM.

Help Support HMEM by donating using the link above.
Tags:
  1. Jul 13, 2018 at 6:51 PM #1

    dkwflight

    dkwflight

    dkwflight

    Active Member

    Joined:
    Sep 4, 2015
    Messages:
    31
    Likes Received:
    10
    I know this is not a model to be shown but
    I think I have read about mixing casting sand with motor oil ( may be used).
    I don't know how well this works but worth a try.

    I do know of a chemical that uses CO2 to harden it, single use.
    Dennis
     
  2. Jul 14, 2018 at 12:09 AM #2

    SmithDoor

    SmithDoor

    SmithDoor

    Well-Known Member

    Joined:
    Feb 12, 2009
    Messages:
    242
    Likes Received:
    35
    I have use Petrobond I use a 30 w oil gear oil
    In mix I use 1% alcohol and petrobond clay
    If looking for good foundry sand look back yard some times that good sand