Search results

Help Support HMEM:

  1. J

    Another PeeWee

    Thourouly dry your casting in the oven Apply loctite 290 (used to be called superwick in) apply pressure /vacuum depending on which is easier to drive the 290 into the casting voids. This will last a lifetime unless you get acetone near it
  2. J

    Leaded steel

    stainless is an extremely poor conductor of heat and electricity which is one of the reasons why it is such a pleasure to weld to prove my point try fusion welding of copper, gas or tig to see what I mean
  3. J

    Leaded steel

    Any proffessional plastics supplier will get it for you It makes Teflon look very cheap